Need Custom Specs?
Contact Us
We supply Plates, Round Bars & Angles cut and processed to your exact size requirements.
Six points architects and fabricators lock down before patina jobs. Your Corten Steel Plate Supplier In India settles them here.
Weathering chemistry decides the patina, so we read the cast sheet first.
Facade panels come off one cast so the rust tones settle evenly.
You are quoted from our own racks with no trading layer added on top.
Cladding gauge and structural plate ship on one invoice, one truck.
Screens, slats and planter blanks are cut here, not sent outside.
Documents travel with the container instead of chasing it later.
Kanakratna Metal Industries stocks both Corten weathering grades. Cladding gauge starts 0.8mm, heavy plate runs to 100mm. Every cast is checked for copper, chromium and phosphorus. Loads leave our Vadodara yard within five working days.
Weathering steel is bought for finish, not only strength. Panels for one elevation come off a single cast. Surface ships as rolled, pickled, blasted or pre-patinated. Corrugated, perforated and slatted profiles are cut in-house.
These clauses decide whether a consignment clears inspection. Check them before your Weathering Steel Plate is dispatched.
Drawing calls out Corten Steel Sheet Thickness in inches? Send it across and we convert against stock gauges.
Work out plate weight before you raise the enquiry. Enter your cut size, thickness and piece quantity. Get kilograms per piece and total consignment weight.
One weathering family, nine ready formats on the floor. Our Corten Steel Plate Suppliers division cuts every profile.









Architectural and mining buyers in these markets take repeat container loads from us.
Tell us the gauge and panel size - the rate comes back off today's rack, not a printed list.
Ladle analysis limits for the two licensed COR-TEN weathering grades, in weight percent.
| Element | Symbol | COR-TEN A | COR-TEN B |
|---|---|---|---|
| Carbon | C | 0.12 max | 0.19 max |
| Silicon | Si | 0.25 - 0.75 | 0.30 - 0.65 |
| Manganese | Mn | 0.20 - 0.50 | 0.80 - 1.25 |
| Phosphorus | P | 0.07 - 0.15 | 0.035 max |
| Sulphur | S | 0.030 max | 0.030 max |
| Aluminium | Al | 0.015 - 0.06 | 0.020 - 0.06 |
| Vanadium | V | Not specified | 0.02 - 0.10 |
| Copper | Cu | 0.25 - 0.55 | 0.25 - 0.40 |
| Chromium | Cr | 0.50 - 1.25 | 0.40 - 0.65 |
| Nickel | Ni | 0.65 max | 0.40 max |
Guaranteed minimum values for licensed COR-TEN plate and strip on tensile test.
On ASTM routes the guaranteed minimum drops with thickness. Heavy plate must be checked band by band.
| Specification & Thickness | Yield Min | Tensile Min |
|---|---|---|
| ASTM A242 Type 1, up to 19mm | 345 MPa | 480 MPa |
| ASTM A242 Type 1, 19mm to 38mm | 315 MPa | 460 MPa |
| ASTM A242 Type 1, 38mm to 100mm | 290 MPa | 435 MPa |
| ASTM A588, up to 100mm | 345 MPa | 485 MPa |
| ASTM A588, 100mm to 125mm | 315 MPa | 460 MPa |
| ASTM A588, 125mm to 200mm | 290 MPa | 435 MPa |
| IS 11587 WR-Fe 480A, up to 12mm | 345 MPa | 480 MPa |
| IS 11587 WR-Fe 480A, 12mm to 40mm | 325 MPa | 480 MPa |
| IS 11587 WR-Fe 480B, up to 40mm | 345 MPa | 480 MPa |
| IS 11587 WR-Fe 500, up to 12mm | 355 MPa | 500 MPa |
The cross-standard calls we are asked to confirm most often on Cor-Ten Steel Plate tenders.
COR-TEN A sits with S355J0WP, COR-TEN B with S355J2W. These are close commercial matches, not identical chemistries.
Facade contractors and fabrication yards across the GCC and Turkey order to a fixed berth date.
Every architect asks before signing off Corten Steel Sheet Cladding. How long until it looks right, and what stains?
Surface darkens patchily and runoff stains paving below.
Reddish brown layer thickens with each wet cycle.
Oxide seals, darkens deep brown, corrosion rate drops.
Scratches and cut edges re-patinate on their own.
Blasting off scale first gives faster, even colour.
Drip edges and gravel margins catch early runoff.
Industrial air darkens patina faster than rural air. Sheltered soffits patinate slowly because they never get wet. Pre-patinated plate ships when the client cannot wait.
Bare weathering steel still loses metal, just slowly. Add these allowances to one face, per decade. Figures apply to untreated COR-TEN B weathering plate.
Cladding gauge and heavy plate leave on the same truck, so you raise one purchase order.
Weathering steel protects itself only when surfaces fully dry. These six site conditions break that drying cycle. Paint the steel or specify another material instead.
Painted weathering steel is still worth specifying here. The same alloying makes a paint film last longer. Coated Corten stays common in Dubai and Cape Town.
Numbers your workshop needs before cutting the first plate. Its higher carbon equivalent changes how preheat behaves.
Post weld heat treatment is rarely required here. Apply the ranges above only when an authority insists. Warm cold-stored plate before mechanical cutting or forming.
Container packing, fumigation and origin papers are handled by our own desk, not a forwarder.
Standard ex-stock range for Corten Steel Plate Sizes, with cut-to-size available on every gauge listed.
| Parameter | Available Range |
|---|---|
| Sheet & Coil Thickness | 0.8mm - 4mm |
| Plate Thickness | 5mm - 100mm |
| Width | 900mm - 3000mm |
| Length | 2000mm - 12000mm |
| Fixed Panel Sizes | 2500 x 1250mm, 3000 x 1500mm, 3000 x 1110mm corrugated |
| Cutting | Laser, plasma, waterjet and oxy-fuel, zero MOQ on stock gauges |
Weathering plate carries an alloy premium over mild steel. Here is what actually moves the number on a quotation.
Realistic windows from the day your purchase order is confirmed, not best-case marketing figures.
Export-packed consignments move to these destinations against confirmed sailings.
Southeast Asian coverage is set out in full below. Africa, the Gulf and Europe are mapped further above. Rush orders reach our Corten Steel Plate Stockist In India.
Third-party witnessed inspection can be arranged before the plate ever leaves the yard.
Where specifiers pick bare Weathering Steel Sheet over paint. The rust itself is accepted as the finish.
There is no fixed rate — we quote against that day's stock. Grade, thickness and sheet size move the figure most, and surface finish or order tonnage shift it further. Corten sits above plain carbon plate because of its copper and chromium content.
COR-TEN A carries 0.07 to 0.15 percent phosphorus and chromium up to 1.25 percent, and it patinates faster, which is why it is preferred for facades and screens. COR-TEN B carries 0.02 to 0.10 percent vanadium with much lower phosphorus, and it welds better, so it is used on heavy structural plate. Both grades are rated at 345 MPa yield and 485 MPa tensile.
Sheet and coil run from 0.8mm to 4mm, while plate covers 5mm to 100mm. Width goes up to 3000mm and length up to 12000mm, and fixed panel sizes of 2500 x 1250mm and 3000 x 1500mm are also available.
The governing Indian standard is IS 11587:1986, Structural Weather Resistant Steels, covering grades WR-Fe 480A, WR-Fe 480B and WR-Fe 500. WR-Fe 480A matches COR-TEN A chemistry and WR-Fe 480B matches COR-TEN B chemistry, while railway work is ordered against IRSM 41-97 instead.
Patina typically takes 18 to 36 months of wet and dry cycles to fully develop, starting reddish brown and darkening with age. Industrial air darkens it faster than rural air, while sheltered surfaces patinate slowly and unevenly. Blasting or pickling the surface before installation speeds the process up.
Corten should not be left bare in salt-laden coastal air, since chlorides stop the patina from sealing and the steel keeps corroding instead of protecting itself. For sites such as the Gulf, the South African coast or Mombasa, and anywhere Canadian de-icing salt collects, painted weathering steel is the better choice.
Corten weighs 7.85 kg per square metre for every 1mm of thickness, based on the IS 11587 density of 7.85 g per cubic centimetre. A 6mm plate works out to about 47.1 kg per square metre, so a 3000 x 1500mm sheet in 6mm weighs roughly 212 kg.