Drag

Contact info

Location
Vadodara, Gujarat, India

Follow us

Manufacturer of ASTM A387 Grade 91 Plate Since 2022 Contact us now
Ex-Stock Dispatch In 48 Hours
ASTM A387 • UNS K90901 • EN 1.4903 • X10CrMoVNb9-1

ASTM A387 Grade 91 Plate

ASTM A387 Grade 91 Plate Key Specifications

Confirm grade, condition, thickness, and certification early so what arrives matches what was ordered
Standard & UNS
ASTM A387 / SA387 Gr.91 Cl.2 / UNS K90901
Governing specification for 9Cr-1Mo-V pressure vessel plate
EN / Werkstoff Reference
EN 10028-2 X10CrMoVNb9-1 / 1.4903
European flat-product equivalent for elevated temperature service
Alloying Elements
Cr 8.00-9.50 / Mo 0.85-1.05 / V 0.18-0.25 / Nb 0.06-0.10
Heat analysis limits per ASTM A387/A387M for Grade 91
Size Range
6mm to 120mm+ Thickness
Width to 3000mm, length to 13000mm, cut-to-size on request
Condition
Normalized & Tempered (N+T)
Austenitized 1040-1080°C, tempered 730-800°C
Ex-Stock Dispatch
3 To 6 Working Days
Counted from Vadodara once thickness and testing are frozen
ASTM A387 Grade 91 Plate

What Ships In Every ASTM A387 Grade 91 Plate Consignment

Boiler fabricators and EPC contractors trust our Vadodara supply. We deliver consistent, code-correct SA 387 Gr.91 Cl.2 Plate

585-760 MPa Class 2 Band

Tensile Confirmed Before Release

Tension tested against Cl.2 window before dispatch.

Cr-Mo-V Verified Per Cast

Heat Number Linked To Plate

Composition results linked to each heat number.

Heavy Section Range Ready

Hot Rolled, Clad And Cut Plate

Boiler and reactor-grade thicknesses always in stock.

Grade Sorted Before Loading

PMI Check On Every Plate

PMI keeps Grade 91 separate from Grade 22.

N+T Records Kept Ready

Normalizing And Tempering Charts

Heat treatment logs travel with every plate.

Cut To Client Drawing

Profile, Bevel Or Flame Cut

Edge prep finished to save site setup time.

Quick answer: ASTM A387 Grade 91 Plate follows SA 387 Gr.91 Cl.2. It reaches 415 MPa yield and 585-760 MPa tensile. Chromium runs 8-9.5%, molybdenum 0.85-1.05%, with vanadium-niobium reinforcement. Suits boilers, reactors and headers running near 600°C.
 

SA 387 GR.91 CL.2 Chrome Moly Plate Supplier in India With MTC

Kanakratna Metal Industries holds ASTM A387 Grade 91 Plate from 6mm to 120mm-plus. All plates ship normalized and tempered. Each carries a heat number for tensile and chemistry results. This backs our role as an SA 387 Gr.91 Cl.2 supplier in Vadodara. Thicker sections beyond stock come through scheduled rolling batches. Hot rolled, clad and cut forms stay stocked separately. Dispatch usually takes three to six working days.

Grade 91 behaves differently from plain Cr-Mo grades like Grade 11 or 22. Its narrow heat window governs vanadium-niobium carbonitride formation for creep strength. Fabrication therefore needs disciplined preheat and post-weld heat treatment control. We share verified chemistry, mechanical data and welding guidance for this grade. This helps your QA team set correct acceptance windows early. Contact us for stock availability and an instant Vadodara quote.

Specification Of ASTM A387 Grade 91 Plate

Buyers often skip essential test fields on enquiries. Our Vadodara ASTM A387 Grade 91 Plate supplier team confirms them

ASTM A387 Grade 91 Plate Specification

SA 387 Gr.91 Radiographic Testing

  • RT offered per ASME Section VIII Div.1
  • Called for boiler drum and reactor shell orders

UNS K90901 Positive Material Identification

  • Handheld XRF reading logged per plate
  • Separates Grade 91 from Grade 22 before loading

Sub-Zero Charpy Impact Option

  • Notch toughness tested when purchaser invokes UG-84
  • Reported alongside the mill test certificate

Grade 91 Plate Product Analysis Option

  • Composition re-checked off the finished plate
  • Ordered when heat analysis alone is not accepted

Carbon Equivalent Reporting

  • CE value stated alongside heat chemistry
  • Used by fabricators to set preheat before welding

Third-Party Inspection Coordination

  • Lloyd's, TUV, BV, SGS and DNV witnessed on request
  • Booked ahead of the planned dispatch window

SA 387 Gr.91 Plate Types

The same 9Cr-1Mo-V chemistry ships in several product forms. A trusted ASTM A387 Grade 91 Plate Manufacturer supplies them all across India

SA 387 Gr 91 Cl2 Normalized & Tempered Plate

SA 387 Gr 91 Cl2 Normalized & Tempered Plate

  • Mandatory heat treatment route for Grade 91
  • Delivers the specified 415 MPa yield floor
A387 Grade 91 Quenched & Tempered Plate

A387 Grade 91 Quenched & Tempered Plate

  • Accelerated cooling route permitted by purchaser agreement
  • Chosen for heavier section thicknesses
SA 387 Grade 91 Boiler Quality Plate

SA 387 Grade 91 Boiler Quality Plate

  • Held for drum and header fabrication work
  • Supplied with full chemistry and hardness data
ASTM A387 Gr 91 Pressure Vessel Quality Plate

ASTM A387 Gr 91 Pressure Vessel Quality Plate

  • Ordered against ASME Section VIII Div.1 shells
  • Radiography and impact data available on request
UNS K90901 Heavy Plate

UNS K90901 Heavy Plate

  • Thicker sections rolled for reactor shell work
  • Ultrasonic scanning available before dispatch
ASTM A387 Grade 91 Profile Cut Plate

ASTM A387 Grade 91 Profile Cut Plate

  • Flame or plasma cut to your drawing outline
  • Reduces fabrication shop machining load
Clad Plate

A387 Grade 91 Clad Plate

  • Corrosion resistant overlay bonded to the base plate
  • Common pick for sour service reactor internals
SA 387 Gr 91 Hot Rolled Plate

SA 387 Gr 91 Hot Rolled Plate

  • Base mill finish ahead of heat treatment
  • Priced separately from finish-machined stock

ASTM A387 Grade 91 Plate Price Factors

Alloy surcharge and testing scope move this grade's price more than base steel rate alone.

Base Alloy Steel Rate
Chromium-Molybdenum-Vanadium Surcharge
Thickness And Section Weight
Normalizing And Tempering Batch Cost
Testing Scope: RT, Impact, TPI
Profile Or Bevel Cutting
Order Tonnage
Delivery Point
A printed Grade 91 plate rate goes stale fast. Alloy surcharge, heat treatment batch size and testing scope all move the number. Send thickness, quantity and testing needs for today's ex-Vadodara rate.

Delivery Estimate For SA 387 Gr.91 Cl.2 Plate

Transit timing across each mode keeps every ASTM A387 Grade 91 Plate order landing on schedule.

Ex-Stock DispatchCleared within 3 to 6 working days once thickness is locked.
Sea Freight20 to 35 days depending on port pairing and vessel booking.
Air Freight4 to 7 days reserved for urgent shutdown work.
Country-Specific ETAConfirmed only once booking and destination port are fixed.

SA 387 Gr.91 Cl.2 Plate Demand Across The Gulf & Turkey

Refinery EPC contractors and boiler fabricators keep returning to our ASTM A387 Grade 91 Plate Supplier in India.

Middle East, Turkey & GCC UAE Saudi Arabia Turkey Qatar
Dubai, UAE
Jubail, Saudi Arabia
Istanbul, Turkey
Doha, Qatar
Abu Dhabi, UAE
Riyadh, Saudi Arabia

ASTM A387 Grade 91 Plate Manufactured At Our Vadodara Facility Since 2022

Share your thickness and testing requirements, and we lock the production route before order confirmation.

Request Quote Now

Refer A387 Gr 91 Class 1 vs Class 2 Plate, Composition and Weight Chart

 

Grade 91 Type 1 Vs Type 2 Chemistry

There's no "Class 1" for Grade 91 — ASTM A387 only lists Class 2. The real choice is Type 1 vs Type 2 chemistry.

T1
Standard Grade 91 chemistry range
T2
Tighter limits for better creep resistance
CL
Only Class 2 tensile is published

At 7.85 g/cm³ density: 10mm weighs ~78.5 kg/m², 20mm ~157 kg/m², 50mm ~392.5 kg/m², 100mm ~785 kg/m².

SA 387 Grade 91 Chemical Composition

Limits shown originate from ASTM A387/A387M for Grade 91, with iron filling the remaining percentage.

ElementSymbolComposition (%)
CarbonC0.08 - 0.12
ManganeseMn0.30 - 0.60
SiliconSi0.20 - 0.50
ChromiumCr8.00 - 9.50
MolybdenumMo0.85 - 1.05
VanadiumV0.18 - 0.25
Niobium (Columbium)Nb0.06 - 0.10
NitrogenN0.030 - 0.070
PhosphorusP0.020 Max
SulfurS0.010 Max
IronFeBalance

ASTM A387 Grade 91 Plate Weight Chart

Calculated at 7.85 g/cm³ steel density. Use this to estimate freight and handling before finalizing an order.

Thickness (mm)Weight (kg/m²)Standard Plate, 2000 x 6000mm (kg)
6mm47.10565.20
8mm62.80753.60
10mm78.50942.00
12mm94.201,130.40
16mm125.601,507.20
20mm157.001,884.00
25mm196.252,355.00
32mm251.203,014.40
40mm314.003,768.00
50mm392.504,710.00
63mm494.555,934.60
75mm588.757,065.00
90mm706.508,478.00
100mm785.009,420.00
120mm942.0011,304.00

ASTM A387 Grade 91 Mechanical Properties

Values shown reflect the Class 2 tensile requirements table from ASTM A387/A387M, normalized and tempered condition.

585-760MPa, Class 2 Requirement
Tensile Strength
415MPa Min, 0.2% Offset
Yield Strength
18%Min, In 8in (200mm)
Elongation
250HB Max, Industry Ceiling
Base Metal Hardness

Creep Rupture Strength At Elevated Temperature

Room-temp tensile numbers miss the point, Grade 91 is chosen for creep strength near 600°C

100,000Hrs Rupture Life Basis
Design Reference Point
565-600°C Service Range
Typical Operating Temperature
V-NbCarbonitrides
Source Of Creep Strength

ASTM A387 Grade 91 Plate Demand From African Refineries

Power utilities and refinery contractors import ASTM A387 Grade 91 Plate through African terminals

Africa South Africa Uganda
Secunda, South Africa
Durban, South Africa
Kampala, Uganda

ASTM A387 Grade 91 Plate Stockist In India Serving Ahmedabad Fabricators

Common thicknesses leave immediately from existing inventory, while unusual sizes move straight into rolling.

Request Quote Now

UNS K90901 Material Equivalent Grades

Procurement teams use several designations when ordering ASTM A387 Grade 91 Plate internationally

USA flagUSA - ASTM/ASME

ASTM A387 / SA387 Gr.91 Cl.2

USA flagUSA - UNS

UNS K90901

Europe flagEurope - EN 10028-2

1.4903, X10CrMoVNb9-1

Germany flagGermany - Werkstoff

Werkstoff Nr. 1.4903

United Kingdom flagUK - BS EN Reference

BS EN 10028-2 X10CrMoVNb9-1

Russia flagRussia - GOST Reference

10Kh9MFB

India flagIndia - Reference

UNS K90901 Nominated On Order

Grade 91 Vs Grade 92 Plate

Grade 92 is often confused with Grade 91, the tungsten addition is what separates them.

Key Chemistry Difference

  • Grade 92 adds 1.5-2.0% tungsten to Grade 91's base
  • Boron trace also added for grain boundary strength

Creep Strength

  • Grade 92 offers higher long-term creep rupture strength
  • Used where design life exceeds Grade 91's safe window

Typical Use

  • Grade 91 remains standard for most boiler and reactor plate
  • Grade 92 reserved for ultra-supercritical, higher-pressure duty

Welding Difficulty

  • Both need matched filler and strict PWHT control
  • Grade 92 has an even narrower tempering window

Cost And Availability

  • Grade 91 is more widely stocked and less costly
  • Grade 92 usually moves on indent, not ex-stock

Which To Specify

  • Choose Grade 91 for standard boiler and reactor plate
  • Choose Grade 92 only where design code calls for it

Grade 91 Plate Exports Reaching Canada, Mexico & The USA

Power plant EPCs and refinery crews across the Americas keep sourcing ASTM A387 Grade 91 Plate.

Americas CanadaMexicoUSAVenezuela
Alberta, Canada
Houston, USA
Mexico
Venezuela

ASTM A387 Grade 91 Plate Exporter To Dubai & Houston With MTC

Certification and customs paperwork are finalized before your consignment leaves the yard.

Request Export Quote

Normalizing & PWHT Cycle For Grade 91 Plate

Getting the thermal window right - not just chemistry - delivers real Grade 91 creep performance

Normalizing WindowAustenitized between 1040°C and 1080°C to dissolve carbides fully
Cooling MethodAir cooled after normalizing to form the required martensitic structure
Tempering RangeHeld between 730°C and 800°C to develop tempered martensite
PWHT Minimum SoakCode sets a 705°C minimum post-weld hold per ASME Section VIII
PWHT CeilingHeld near 775°C max so the original tempering is never undone
Delta Ferrite WatchUnder-normalizing below the window risks retained delta ferrite pockets

Grade 91 Plate Shipments Into Southeast Asia

Power and petrochemical EPCs in this region keep ordering ASTM A387 Grade 91 Plate ahead of turnarounds

Southeast Asia SingaporeThailandMalaysiaIndonesia
Singapore
Bangkok, Thailand
Malaysia
Indonesia
Philippines
Vietnam

ASTM A387 Grade 91 Plate Supplier In India With Full EN 10204 3.1 Compliance

Every heat treatment batch stays documented, keeping your inspection paperwork fully traceable.

Get Supplier Quote

Preheat And Interpass Control While Welding Gr.91

Fabricators handling our ASTM A387 Grade 91 Plate plan these thermal checkpoints before striking an arc

PH
Minimum preheat held around 200°C to 204°C before any tack weld
IP
Interpass temperature capped near 300°C between weld passes
HB
Hydrogen bake-out held at 300°C to 350°C for 2 to 4 hours
MF
Weld cooled below roughly 96°C before PWHT begins
FL
Matching B9 filler metal keeps chemistry aligned with the base plate
PG
Interpass and preheat recorded on the weld traveller for every pass

Hardness Acceptance Limits After PWHT

Field hardness checks decide whether an ASTM A387 Grade 91 Plate weld is released or sent back for further tempering.

250 HB Max, Base Metal Ceiling
190 HB Typical Field Floor
265 HV Vickers Cross-Check Limit
Weld & HAZ Checked Alongside Base Metal

Machining And Flame-Cutting Guidance

Grade 91's hardness and heat sensitivity mean cutting and machining need the same discipline as welding.

Preheat Before Flame Cutting150-200°C preheat reduces heat-affected zone cracking risk
Plasma Or Waterjet OptionChosen where minimal heat input to the cut edge matters
MachinabilityRated lower than carbon steel due to chromium-molybdenum content
Bevel PreparationEdge bevels cut to weld procedure specification before dispatch
Post-Cut GrindingRemoves heat-tint and surface hardening from the cut face
Edge InspectionDye penetrant check offered on flame-cut edges before shipping

Construction Codes Referencing A387 Grade 91

Engineers check these codes before releasing a Grade 91 Plate order.

P-No. 5B Group 2

  • Governs welding qualification under ASME IX
  • Sets base material grouping

ASME Section I & VIII Div.1

  • Covers boiler and pressure vessel plate
  • Sets heat treatment and testing rules

API 938B Refining Guidance

  • Notes on using 9Cr-1Mo-V steel
  • Referenced across South Africa and the Gulf

EN 10204 3.1 / 3.2

  • 3.1 standard, 3.2 on nomination
  • Matched to buyer's inspection needs

HSN Code, Export Documentation And Packaging

Classification and packing errors are the most common cause of port delays on this grade

HSN Heading 7225

  • Covers flat-rolled alloy steel products above 600mm width
  • Sub-heading confirmed against actual width and grade

Domestic GST

  • Alloy steel plate attracts 18% GST on Indian supply
  • Confirmed against current CBIC rate before invoicing

Origin And Inspection Papers

  • Certificate of Origin issued via chamber of commerce
  • Third-party inspection certificate attached where nominated

Export Packing

  • Edge-protected bundling to prevent transit corner damage
  • Moisture barrier wrap for long sea-transit routes

Shipping Documents

  • Mill test certificate, packing list and invoice in the container
  • Bill of lading and COO couriered ahead of vessel arrival

Heavy Plate Handling

  • Wooden cradles used for thick, high-tonnage single pieces
  • Lifting lug positions marked on the packing list

Where ASTM A387 Grade 91 Plate Gets Used

Engineering teams reach for our ASTM A387 Grade 91 Plate Manufacturer In India for high-temperature creep resistance

Ultra-Supercritical Boiler HeadersThick sections needing long-term creep strength.
Steam Generator Skirts & SupportsStructural plate around high-temperature drums.
Petrochemical Reactor ShellsVessel walls exposed to sustained process heat.
HRSG Pressure PartsHeat recovery steam generator components.
Refinery Furnace Tube SheetsHigh-temperature process heater components.
Pressure Vessel Heads & ShellsASME Section VIII fabricated equipment.
Superheater Support PlateRetrofit material for cycling power plants.
Advanced Reactor Coolant SystemsStudied for next-generation nuclear plant design.

ASTM A387 Grade 91 Plate Frequently Asked Questions

Is ASTM A387 Grade 91 Plate available in Class 1?
No, ASTM A387 lists Grade 91 only as Class 2
Further split into Type 1 and Type 2 chemistry
Class 1 tensile requirements don't apply to this grade
What is the difference between Grade 91 and Grade 22 plate?
Grade 91 adds vanadium and niobium to 9% chromium
Gives stronger creep resistance near 600°C
Grade 22 uses 2.25% chromium for moderate temperature duty
What is the European equivalent of Grade 91 plate?
EN 10028-2 lists it as grade 1.4903
Chemistry designation X10CrMoVNb9-1
Same 9Cr-1Mo-V family as UNS K90901
What is the ASTM A387 Grade 91 plate price in India?
Depends on thickness, cut size and quantity
Heat treatment batch also affects the rate
Send your size list for a firm ex-Vadodara quote
What heat treatment does Grade 91 plate require?
Austenitized between 1040 and 1080°C
Tempered between 730 and 800°C
Narrower cycle than other A387 grade annealing
Quick Response
Need Pricing Or Stock Info?

Message us directly, we reply fast.

No spam, ever · We usually reply within 2 hours