Six points machinery and boiler-fabrication buyers lock down before a chrome-moly order moves. Your Alloy Steel Plate Supplier In India settles them here.
Each heat is cross-checked against grade chemistry before cutting starts.
Machinery grade and boiler grade ship on one invoice, one truck.
You are quoted from our own racks with no trading layer added on top.
Pressure-vessel chemistry sits alongside machinery-grade plate.
Blanks, rings and flanges are cut here, not sent outside.
Documents travel with the container instead of chasing it later.
Machinery buyers ask for this plate by carbon content - 4140 or 4130 by name. Refinery and boiler buyers ask for it by chromium-molybdenum percentage - Grade 11 or Grade 22. Both families sit on the same Vadodara floor, cut to size against the same purchase order, with chemistry checked against the cast sheet before the plate reaches the shear. We work as an Alloy Steel Plate stockist in India, holding machinery-grade and pressure-vessel-grade chemistry ex-stock together.
4140 and 4340 both call for preheat before welding; A387 Grade 22 calls for it more than Grade 11 given the higher molybdenum content. No plate leaves the yard without its heat-treatment condition confirmed on the packing list - normalized, normalized-and-tempered, or quenched-and-tempered. We operate as an Alloy Steel Plate supplier in Vadodara, serving boiler fabricators and machinery shops from the same rack.
Cross-standard reading most buyers ask for before the PO is cut, across both the machinery family and the A387 Cr-Mo pressure-vessel family.
Chemistry ranges are close, not identical, across standards. Confirm the exact designation your buyer's drawing calls for before order confirmation.
Refinery, EPC and boiler-fabrication buyers across the GCC and Turkey book against a fixed berth date. We are trusted Alloy Steel Plate Suppliers in Saudi Arabia, shipping Cr-Mo plate directly to Riyadh.
Tell us the grade and heat-treatment condition - the rate comes back off today's rack, not a printed list.
Heat analysis limits in weight percent, machinery grades against the two most-ordered A387 Cr-Mo grades.
| Element | 4140 | 4130 | 4340 | A387 Gr.11 | A387 Gr.22 |
|---|---|---|---|---|---|
| Carbon (C) | 0.38-0.43 | 0.28-0.33 | 0.38-0.43 | 0.04-0.17 | 0.04-0.15 |
| Manganese (Mn) | 0.75-1.00 | 0.40-0.60 | 0.60-0.80 | 0.35-0.73 | 0.25-0.66 |
| Silicon (Si) | 0.15-0.35 | 0.15-0.35 | 0.15-0.35 | 0.44-0.86 | 0.50 max |
| Chromium (Cr) | 0.80-1.10 | 0.80-1.10 | 0.70-0.90 | 0.94-1.56 | 1.88-2.62 |
| Molybdenum (Mo) | 0.15-0.25 | 0.15-0.25 | 0.20-0.30 | 0.40-0.70 | 0.85-1.15 |
| Nickel (Ni) | - | - | 1.65-2.00 | - | - |
| Phosphorus (P) | 0.035 max | 0.035 max | 0.035 max | 0.035 max | 0.035 max |
| Sulphur (S) | 0.040 max | 0.040 max | 0.040 max | 0.035 max | 0.035 max |
4130 carries less carbon than 4140 for easier welding at some cost to through-hardening. Grade 22 carries roughly double the molybdenum of Grade 11 for better creep strength at temperature. Confirm the cast sheet against your buyer's own spec before order confirmation.
Clauses checked before dispatch.
Rockwell or Vickers on drawing? We cross-check against the guaranteed tensile figure.
Two chemistry families, nine ready formats on the floor. Our Alloy Steel Plate Suppliers division cuts every profile.









Power, cement and process-equipment fabricators across these markets take repeat container bookings from us. As an established Alloy Steel Plate exporter, our own desk handles packing and origin papers.
Container packing, fumigation and origin papers run through our own desk, not a forwarder.
Typical values by grade and supplied condition - tensile and yield move sharply with heat-treatment condition on the SAE grades.
A387 figures are guaranteed ASTM minimums. SAE 4140/4130/4340 figures are typical mill values - always confirm against the certified test report for load-critical parts.
| Grade | Condition | Tensile Strength | Yield Strength | Elongation |
|---|---|---|---|---|
| 4140 | Quenched & Tempered | 850-1000 MPa | 670 MPa min | 15-20% |
| 4130 | Normalized | 670 MPa approx | 435 MPa approx | 25% approx |
| 4340 | Quenched & Tempered | 860-1980 MPa | 740-1860 MPa | 11-23% |
| A387 Gr.11 Cl.2 | Normalized & Tempered | 515-690 MPa | 310 MPa min | 18% min |
| A387 Gr.22 Cl.2 | Normalized & Tempered | 515-690 MPa | 310 MPa min | 18% min |
Condition changes the delivered strength more than the grade name does - state it on the PO, do not leave it to the mill's default.
| Grade | Normalizing / Austenitizing | Minimum Temper |
|---|---|---|
| 4140 | 840-875°C, oil or water quench | 550-700°C per required hardness |
| 4130 | 815-870°C, oil quench | 400-565°C per required hardness |
| A387 Gr.11 | Normalized, or accelerated cool if agreed | 621°C (1150°F) minimum |
| A387 Gr.22 | Normalized, or accelerated cool if agreed | 677°C (1250°F) minimum |
Class 1 tensile level on A387 plate typically ships normalized and tempered; Class 2 typically ships quenched and tempered for the higher strength band. Chemistry stays the same across both classes.
Refinery and machinery-shop consignments move to these destinations against confirmed sailings.
Third-party witnessed inspection can be arranged before the plate ever leaves the yard.
A387 Gr.11 and Gr.22 are selected per API RP 941 Nelson curves for elevated-temperature and hydrogen service. 4140/4130/4340 machinery grades are not rated for sustained creep above roughly 370°C.
Standard window for A387 grades
Governs Cr-Mo choice in hydrogen duty
Confirms chemistry hasn't drifted
Full Grade 11 vs Grade 22 comparison is covered on our dedicated A387 grade page
Canadian and cold-climate fabricators raise this before wear or strength questions. Neither family is cold-rated by default.
| Behaviour In Deep Cold | 4140 / 4130 / 4340 | A387 Gr.11 / Gr.22 |
|---|---|---|
| Standard Charpy Data | Not included unless ordered | Not included unless ordered |
| Notch Sensitivity | Rises with hardness and temper level | Low carbon content keeps it manageable |
| Cold-Rated Variant | Fine-grain practice available on request | Impact-tested variant available on request |
Not tested unless PO states it
Confirm lot-availability before date
Avoids mismatch once plate ships
Lower carbon eases field welding
Carbon and alloy content raise crack risk on every grade here - preheat and PWHT are shop practice, not an optional step.
| Grade | Typical Preheat | Typical PWHT |
|---|---|---|
| 4140 | 150-260°C | Stress relieve 595-675°C |
| 4130 | 95-150°C | Lower carbon eases the requirement |
| 4340 | 150-260°C | Stress relieve 595-675°C |
| A387 Gr.11 | Per WPS, typically 150°C+ | Mandatory above code-set thickness |
| A387 Gr.22 | Per WPS, typically 200°C+ | Mandatory, higher alloy needs tighter control |
Figures are shop planning guidance - confirm the exact preheat and PWHT band against your qualified WPS and the governing code.
Standard ex-stock range across the full Alloy Steel Plate family, with cut-to-size available on every gauge listed.
| Parameter | Available Range |
|---|---|
| Plate Thickness | 5mm - 200mm |
| Width | Up to 2500mm |
| Length | Up to 12000mm |
| Fixed Panel Sizes | 2500 x 1250mm, 2000 x 6000mm |
| Cutting | Plasma, oxy-fuel and machining, zero MOQ on stock gauges |
HSN classification and applicable GST for billing on domestic orders.
| Product | HSN Code | GST Rate |
|---|---|---|
| Alloy Steel Plate (width 600mm & above) | 7225 | 18% |
| Alloy Steel Plate / Strip (width below 600mm) | 7226 | 18% |
HSN code can shift with exact width and finish - confirm against your GST invoice requirement before order confirmation.
Chrome-moly chemistry carries an alloy premium over carbon steel. Here is what actually moves the number on a quotation.
Higher Mo grades like Gr.22 cost more
Heavier gauge raises per-kg rate
Q&T costs more than normalized
3.1 certification adds to base rate
UT/PMI add inspection charges
Higher volume improves per-kg pricing
Fumigated wooden crates add cost
Freight varies by destination port
Counted from the day the PO is confirmed, not the enquiry date.
Estimate only - confirmed sailing dates follow booking.
Southeast Asian coverage is set out below. Africa, the Gulf and Europe are mapped further above. Rush orders reach our Alloy Steel Plate Stockist In Vadodara direct.
Send the grade, thickness and heat-treatment condition - we confirm chemistry against the application before the plate leaves the yard.
Where chrome-moly chemistry earns the premium over carbon steel.
A387 Gr.11/Gr.22 elevated-temperature duty
Cr-Mo chemistry for process heat service
4140/4130 for oil and gas drilling gear
4140/4340 for high-torque machinery parts
4340 for aerospace and heavy-duty parts
Grade 22 for hydrogen-service vessels
Elevated-temperature steam circuit components
Custom-cut blanks for any design
No fixed rate - grade, thickness, heat-treatment condition and tonnage move the figure most.
4140 carries more carbon for higher strength; 4130 carries less carbon and welds more easily.
Closest match is EN 13CrMo4-5 under EN 10028-2, same 1.25Cr-0.5Mo family.
5mm to 200mm ex-stock across 4140, 4130, 4340 and A387 Gr.11/Gr.22 chemistry.
Yes, with correct preheat and PWHT - carbon and alloy content make skipping either risky.